Material: Stucco
Condition: Crack Repair Failed
TPAS Code: CRprF
Condition Type (AutoCAD Layer): Stucco_Crack
Severity Units: Not applicable
Ammount Units: Length in lineal feet
Description: A crack or crack system that has been filled using elastomeric, cementitous or other repair material in which the repair material exhibits signs of failure or deterioration.