Material: Stone
Condition: Joints Sealant Failed
TPAS Code: SlntF
Condition Type (AutoCAD Layer): Stone_Joints
Severity Units: Not applicable
Ammount Units: Lineal feet of sealant failed
Description: Joints containing sealant, such as expansion or control joints, in which the sealant exhibits cracking, separation, total loss or other signs of deterioration.